Okay, here’s the gold P-32D after a bit of wet sanding and touch-up. I will now let this cure for at least two months before laying hands on it again. This has multiple layers of Krylon Cover MAXX Metallic Gold over the original finish (after fine steel wool) and then coating with Krylon ColorMaster Acrylic Crystal Clear Gloss. The finish is not as metallic and glossy as it looked at first, having dulled somewhat after about a week of drying/curing. But I probably won’t try to get more of a shine.



I have to say after working with Rust-oleum on the other P-32D and the P-25E (still in process) that it is much easier to get an even and smooth finish with Krylon.